325 stainless steel mesh screen
0.5 mil emulsion
Allow parts to level for 10 – 15 minutes before drying, but
parts should be dried as soon as possible after leveling to
prevent skinning, which can compromise adhesion. Wet
parts should be covered if not dried right away.